冷却速度对Zn--5 Al--0.1 RE--x Si合金显微组织及耐蚀性能的影响
引用本文:涂浩,魏大圣,周圣洁,刘亚,吴长军,苏旭平,王建华. 冷却速度对Zn--5 Al--0.1 RE--x Si合金显微组织及耐蚀性能的影响[J]. 北京科技大学学报, 2016, 0(8): 1132-1138. DOI: 10.13374/j.issn2095-9389.2016.08.012
作者姓名:涂浩  魏大圣  周圣洁  刘亚  吴长军  苏旭平  王建华
作者单位:1. 常州大学材料科学与工程学院,常州213164; 常州大学江苏省材料表面科学与技术重点实验室,常州213164;2. 常州大学材料科学与工程学院,常州213164; 常州大学江苏省材料表面科学与技术重点实验室,常州213164; 常州大学江苏省光伏科学与工程协同创新中心,常州213164
基金项目:国家自然科学基金资助项目(51271040
摘    要:运用扫描电子显微镜/能谱仪、X射线衍射、盐雾实验、电极化曲线等手段,研究冷却速度和Si对Zn-5Al-0.1RE合金组织及耐蚀性能的影响.结果表明,Zn-5Al-0.1RE-xSi合金由先析出的?-Zn和?-Zn+α-Al共晶组织组成,前者均匀分布在相邻的?-Zn+α-Al共晶胞的边界上.降低冷却速度和Si的加入,均使Zn-5Al-0.1RE-xSi合金单位面积的晶粒增大,晶界减少,合金耐蚀性能提高. Zn-5Al-0.1RE-xSi合金耐蚀性能的差异与合金凝固组织及合金腐蚀产物中Zn5(OH)8Cl2·H2O和ZnO的相对量有关.

关 键 词:锌铝合金  冷却速度  微观结构  耐蚀性能    热浸镀锌

Effect of cooling rate on the microstructure and corrosion properties of Zn--5Al--0. 1RE--xSi alloys
TU Hao,WEI Da-sheng,ZHOU Sheng-jie,LIU Ya,WU Chang-jun,SU Xu-ping,WANG Jian-hua. Effect of cooling rate on the microstructure and corrosion properties of Zn--5Al--0. 1RE--xSi alloys[J]. Journal of University of Science and Technology Beijing, 2016, 0(8): 1132-1138. DOI: 10.13374/j.issn2095-9389.2016.08.012
Authors:TU Hao  WEI Da-sheng  ZHOU Sheng-jie  LIU Ya  WU Chang-jun  SU Xu-ping  WANG Jian-hua
Abstract:The effects of cooling rate and Si on the microstructure and corrosion property of the Zn-5Al-0. 1RE alloy were studied by scanning electron microscopy-energy dispersive spectrometry, X-ray diffraction, neutral salt spray test and polarization curves. The results show that Zn-5Al-0. 1RE-xSi alloys are composed of primary?-Zn phase and ?-Zn+α-Al eutectic structure, and the former is uniformly distributed on the adjacent ?-Zn+α-Al eutectic cells. The reduction of cooling rate and the addition of Si make the grain size increase and the boundary area per unit alloy area decrease;at the same time, the corrosion resistance is improved. The corrosion resistance of the Zn-5Al-0. 1RE-xSi alloys is dependent on their solidification structure and the relative amount of corrosion products including Zn5 ( OH) 8 Cl2·H2 O and ZnO.
Keywords:zinc aluminum alloys  cooling rate  microstructure  corrosion resistance  silicon  hot dip galvanizing