首页 | 本学科首页   官方微博 | 高级检索  
     

溶液共混法制备PET/纳米SiO2复合材料
引用本文:邓建国,李新跃. 溶液共混法制备PET/纳米SiO2复合材料[J]. 四川理工学院学报(自然科学版), 2008, 21(2): 112-114
作者姓名:邓建国  李新跃
作者单位:四川理工学院材料与化学工程系,四川,自贡,643000;四川理工学院材料与化学工程系,四川,自贡,643000
摘    要:纳米SiO2具有异相成核的作用,能提高PET的结晶能力。文章探讨了溶液共混法和不同偶联剂对PET结晶能力的影响。结果表明:悬浮液的PH=9~10时,分散均匀性最好;采用溶液共混法进行复合,可制得熔点低于纯PET熔点的PET树脂/纳米SiO2复合材料。

关 键 词:溶液共混法  纳米SiO2  PET
文章编号:1673-1549(2008)02-0112-03
修稿时间:2007-08-14

Preparation of PET/Nano-SiO2 Composite Materials by Solution Co-blending Method
DENG Jian-guo,LI Xin-yue. Preparation of PET/Nano-SiO2 Composite Materials by Solution Co-blending Method[J]. Journal of Sichuan University of Science & Engineering(Natural Science Editton), 2008, 21(2): 112-114
Authors:DENG Jian-guo  LI Xin-yue
Abstract:Nano-SiO2 has a kind of property of forming nucleation during different direct,which can improve the crystallization of PET.In this paper,solution co-blending method and different coupling agents were discussed to understand them how to effect the crystallization of PET.The results indicated that Nano-SiO2 could be dispersed effectively when the pH value of suspension is 9 to 10.Besides,we can get PET resins/Nano-SiO2 composite materials which has lower melt point than PET when solution co-blending method was applied.
Keywords:solution co-blending method  Nano-SiO2  PET