Preparation and properties of thermal insulation coatings with a sodium stearate-modified shell powder as a filler
Authors:Qiang Tang  Ya-mei Zhang  Pei-gen Zhang  Jin-jie Shi  Wu-bian Tian  Zheng-ming Sun
Institution:1. Jiangsu Key Laboratory of Construction Materials,School of Materials Science and Engineering,Southeast University,Nanjing 211189,China;2. Jiangsu Key Laboratory of Advanced Metallic Materials,School of Materials Science and Engineering,Southeast University,Nanjing 211189,China
Abstract:Waste shell stacking with odor and toxicity is a serious hazard to our living environment. To make effective use of the natural re-sources, the shell powder was applied as a filler of outdoor thermal insulation coatings. Sodium stearate (SS) was used to modify the proper-ties of shell powder to reduce its agglomeration and to increase its compatibility with the emulsion. The oil absorption rate and the spectrum reflectance of the shell powder show that the optimized content of SS as a modifier is 1.5wt%. The total spectrum reflectance of the coating made with the shell powder that is modified at this optimum SS content is 9.33% higher than that without any modification. At the optimum SS content of 1.5wt%, the thermal insulation of the coatings is improved by 1.0℃ for the cement mortar board and 1.6℃ for the steel plate, respectively. The scouring resistance of the coating with the 1.5wt% SS-modified shell powder is three times that of the coating without modification.
Keywords:heat insulation coatings  shell powder  sodium stearate  scrub resistance
本文献已被 万方数据 SpringerLink 等数据库收录!
点击此处可从《矿物冶金与材料学报》浏览原始摘要信息
点击此处可从《矿物冶金与材料学报》下载免费的PDF全文
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号