Recovery of iron from copper tailings via low-temperature direct reduction and magnetic separation: process optimization and mineralogical study
Authors:Rui-min Jiao  Peng Xing  Cheng-yan Wang  Bao-zhong Ma  Yong-Qiang Chen
Institution:School of Metallurgical and Ecological Engineering, University of Science and Technology Beijing, Beijing 100083, China
Abstract:Currently,the majority of copper tailings are not effectively developed.Worldwide,large amounts of copper tailings generated from copper production are continuously dumped,posing a potential environmental threat.Herein,the recovery of iron from copper tailings via low-temperature direct reduction and magnetic separation was conducted;process optimization was carried out,and the corresponding mineralogy was investigated.The reduction time,reduction temperature,reducing agent (coal),calcium chloride additive,grinding time,and magnetic field intensity were examined for process optimization.Mineralogical analyses of the sample,reduced pellets,and magnetic concentrate under various conditions were performed by X-ray diffraction,optical microscopy,and scanning electron microscopy-energy-dispersive X-ray spectrometry to elucidate the iron reduction and growth mechanisms.The results indicated that the optimum parameters of iron recovery include a reduction temperature of 1150℃,a reduction time of 120 min,a coal dosage of 25%,a calcium chloride dosage of 2.5%,a magnetic field intensity of 100 mT,and a grinding time of 1 min.Under these conditions,the iron grade in the magnetic concentrate was greater than 90%,with an iron recovery ratio greater than 95%.
Keywords:copper tailings  iron  direct reduction  magnetic separation  recovery  process optimization
本文献已被 万方数据 SpringerLink 等数据库收录!
点击此处可从《矿物冶金与材料学报》浏览原始摘要信息