摘    要:为研究正交胶合木(CLT)楼板炭化速度有限元分析方法,在ISO834标准升温条件下进行了3组国产CLT楼板的火灾试验。对胶黏层的拉伸与剪切试验进行有限元模拟,建立了2种CLT楼板炭化速度有限元模型,即未考虑层板脱落和考虑层板脱落的有限元模型。将试验得到的温度-时间曲线、炭化深度(速度)曲线与有限元模型的模拟结果进行对比。研究结果表明,受火时间越长,炭化速度越大;采用胶黏单元来模拟CLT板中的胶黏剂是可行的;考虑层板脱落的炭化速度有限元模拟结果与试验得到的炭化速度结果吻合较好。

关 键 词:正交胶合木  炭化速度  胶黏剂  有限元  层板脱落
收稿时间:2019-11-03

Finite Element Analysis of the Charring Rate of Cross-Laminated Timber Floor
ZHANG Jin,CHEN Hao,BAI Yu,LIAO Jianan. Finite Element Analysis of the Charring Rate of Cross-Laminated Timber Floor[J]. Journal of Tongji University(Natural Science), 2020, 48(8): 1122-1131
Authors:ZHANG Jin  CHEN Hao  BAI Yu  LIAO Jianan
Affiliation:1.Key Laboratory of Concrete and Prestressed Concrete Structures of the Ministry of Education, Southeast University, Nanjing 211189, China;2.Organizing Committee of Nanning New and Hi-Tech Industry Development Zone, Nanning 530007, China
Abstract:In order to study the finite element analysis method of charring rate of cross-laminated timber (CLT) floor, three groups of domestic CLT floor fire experiments were conducted under ISO834 standard temperature rising conditions. Tensile and shear tests of the adhesive layer were simulated by using the finite element method, and two kinds of finite element models of charring rate of CLT floor were established: the finite element model without considering the delamination of the laminate and that considering the delamination of the laminate. The temperature-time curve and charring depth (rate) curve obtained from the test data were compared with the simulation results of the finite element model.The results show that the longer the fire time is, the higher the charring rate is.Besides, it is feasible to simulate the adhesive in the CLT plate by using cohesive element.Moreover, the finite element simulation results of the carbonization rate considering the delamination of the laminates agree well with the results of the carbonization rate obtained by the test.
Keywords:cross-laminated timber(CLT)  charring rate  adhesive  finite element  delamination
本文献已被 CNKI 等数据库收录!
点击此处可从《同济大学学报(自然科学版)》浏览原始摘要信息
点击此处可从《同济大学学报(自然科学版)》下载全文
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号