摘    要:采用活化溅射方法,在不同溅射电压条件下,在NiTi形状记忆合金表面成功制备出了纳米TiO2生物薄膜.采用台阶轮廓仪和拉曼光谱仪研究溅射电压对薄膜厚度和晶体结构的影响,并对NiTi合金覆膜前后在37℃模拟人体体液中的耐腐蚀性能进行了评价.结果表明,在本实验条件下薄膜为锐钛矿结构,薄膜表面均匀,其主要成分为纳米尺寸的TiO2;TiO2薄膜明显改善了NiTi合金在37℃模拟人体体液中的耐腐蚀性能.

关 键 词:NiTi形状记忆合金  活化溅射  TiO2薄膜  溅射电压  

Preparation of TiO2 Thin Biofilm on NiTi Alloy by Activation Sputtering Method
GAO Shu-chun,ZHAI Yu-chun,JIANG Da,WANG Qiu-shi. Preparation of TiO2 Thin Biofilm on NiTi Alloy by Activation Sputtering Method[J]. Journal of Northeastern University(Natural Science), 2013, 34(6): 859-862
Authors:GAO Shu-chun  ZHAI Yu-chun  JIANG Da  WANG Qiu-shi
Affiliation:1(1.School of Materials & Metallurgy,Northeastern University,Shenyang 110819,China;2.School of Materials Science and Engineering,Shenyang Aerospace University,Shenyang 110136,China
Abstract:Based on different sputtering voltage conditions, nanometer titanium dioxide bio film was prepared on NiTi shape memory alloy surface by the activation sputtering method. The influences of the sputtering voltage on the thickness of the film and crystal structure were studied by the step profiler and Raman spectrum. The corrosion resistance of the NiTi alloy and TiO2 coated NiTi alloy was evaluated in simulated body fluid at 37℃, respectively. Results showed that under the condition of this experiment the thin film was anatase structure, and the major constituent was nanometer titanium dioxide. The titanium dioxide thin films effectively improved the corrosion resistance of the NiTi alloy in simulated body fluid at 37℃.
Keywords:NiTi shape memory alloy  activation sputtering  TiO2 thin films  sputtering voltage