Kinetics of thermal decomposition of hydrated minerals associated with hematite ore in a fluidized bed reactor
Authors:P. C. Beuria  S. K. Biswal  B. K. Mishra  G. G. Roy
Affiliation:1.Institute of Minerals and Materials Technology,Council of Scientific & Industrial Research,Bhubaneswar,India;2.Indian Institute of Technology,Kharagpur,India
Abstract:The kinetics of removal of loss on ignition (LOI) by thermal decomposition of hydrated minerals present in natural iron ores (i.e., kaolinite, gibbsite, and goethite) was investigated in a laboratory-scale vertical fluidized bed reactor (FBR) using isothermal methods of kinetic analysis. Experiments in the FBR in batch processes were carried out at different temperatures (300 to 1200°C) and residence time (1 to 30 min) for four different iron ore samples with various LOIs (2.34wt% to 9.83wt%). The operating velocity was maintained in the range from 1.2 to 1.4 times the minimum fluidization velocity (U mf). We observed that, below a certain critical temperature, the FBR did not effectively reduce the LOI to a desired level even with increased residence time. The results of this study indicate that the LOI level could be reduced by 90% within 1 min of residence time at 1100°C. The kinetics for low-LOI samples (<6wt%) indicates two different reaction mechanisms in two temperature regimes. At lower temperatures (300 to 700°C), the kinetics is characterized by a lower activation energy (diffusion-controlled physical moisture removal), followed by a higher activation energy (chemically controlled removal of LOI). In the case of high-LOI samples, three different kinetics mechanisms prevail at different temperature regimes. At temperature up to 450°C, diffusion kinetics prevails (removal of physical moisture); at temperature from 450 to 650°C, chemical kinetics dominates during removal of matrix moisture. At temperatures greater than 650°C, nucleation and growth begins to influence the rate of removal of LOI.
Keywords:
本文献已被 万方数据 SpringerLink 等数据库收录!
点击此处可从《矿物冶金与材料学报》浏览原始摘要信息
点击此处可从《矿物冶金与材料学报》下载免费的PDF全文