首页 | 本学科首页   官方微博 | 高级检索  
     检索      

N80-1套管失效分析
引用本文:邹喜洋,付茂林.N80-1套管失效分析[J].南华大学学报(自然科学版),2007,21(2):75-78.
作者姓名:邹喜洋  付茂林
作者单位:1. 湖南衡阳华菱钢管有限公司,湖南,衡阳,421001
2. 南华大学,数理学院,湖南,衡阳,421001
摘    要:简述了非调质N80套管存在的问题,分析了用非调质钢36Mn2V制造的N80套管在油田失效的原因,并提出了改进措施.

关 键 词:非调质钢  套管  脆性  在线常化
文章编号:1673-0062(2007)02-0075-04
收稿时间:2007-03-14
修稿时间:2007-03-14

Failure Analysis of N80-1 Casing
ZOU Xi-yang,FU Mao-lin.Failure Analysis of N80-1 Casing[J].Journal of Nanhua University:Science and Technology,2007,21(2):75-78.
Authors:ZOU Xi-yang  FU Mao-lin
Institution:1. Hunan Hengyang Valin Steel Tube Co. Ltd. , Hengyang, Hunan 421001, China ;2. School of Mathematics and Physics Science,University of South China,Hengyang,Hunan 421001 ,China
Abstract:The problem of non-quenched and tempered N80 casing is stated simply.Failure reason of N80 casing made of non-quenched and tempered steel 36Mn2V is analysized,and the way of improvement is given.
Keywords:non-quenched and tempered steel  casing  brittleness  on-line normalization
本文献已被 CNKI 维普 万方数据 等数据库收录!
点击此处可从《南华大学学报(自然科学版)》浏览原始摘要信息
点击此处可从《南华大学学报(自然科学版)》下载免费的PDF全文
设为首页 | 免责声明 | 关于勤云 | 加入收藏