Z. Orságová Králová R. Gorejová R. Oriňaková M. Petráková A. Oriňak M. Kupková M. Hrubovčáková T. Sopčák M. Baláž I. Maskaľová A. Kovalčíková K. Kovaľ 《自然科学进展(英文版)》2021,31(2):279-287
Zn-Fe alloys have been extensively investigated in this study with a view to their application as biodegradable bone implants. Biogenic element zinc is a very appropriate metal because of the ideal degradation rate compared to those of Mg and Fe. Studied alloys were made by compressing metallic powders in a content ratio of 100% Zn,Zn-1% Fe, Zn-2% Fe, Zn-5% Fe and Zn-10% Fe and sintering at 350°C for 1 h. Prepared samples were examined by optical microscopy, SEM and XRD. Corrosion behavior, mechanical testing and hemocompatibility were observed subsequently. The electrochemical performance of such materials was studied in the simulated body fluids. The enhanced corrosion rate was observed for all samples after iron addition due to the micro-galvanic effect between the pure Zn and Zn_(11)Fe intermetallic phase. The corrosion rate of the Zn-5% Fe alloyed sample was more than 20-times higher(2.89 mmpy) compared to the pure Zn. However, alloying with more than 5 wt %of iron diminished the mechanical performance of the material. Therefore, the performed mechanical and hemocompatibility tests showed acceptable biocompatibility of zinc and Zn-1% Fe and Zn-2% Fe samples. 相似文献
52.
Adel Alahmadi Husain Alhazmi Shakir Ali Tor Helleseth Rola Hijazi Chunlei Li Patrick Solé 《系统科学与复杂性》2017,30(4):950-966
This paper constructs a cyclic ?4-code with a parity-check matrix similar to that of Goethals code but in length 2m + 1, for all m ≥ 4. This code is a subcode of the lifted Zetterberg code for m even. Its minimum Lee weight is shown to be at least 10, in general, and exactly 12 in lengths 33, 65. The authors give an algebraic decoding algorithm which corrects five errors in these lengths for m = 5, 6 and four errors for m > 6. 相似文献