1.
The iron concentrate from Hercules Mine of Coahuila, Mexico, which mainly contained pyrite and pyrrhotite, was treated by the bioleaching process using native strain Acidithiobacillus ferrooxidans (A. ferrooxidans) to determine the ability of these bacteria on the leaching of zinc. The native bacteria were isolated from the iron concentrate of the mine. The bioleaching experiments were carried out in shake flasks to analyze the effects of pH values, pulp density, and the ferrous sulfate concentration on the bioleaching process. The results obtained by microbial kinetic analyses for the evaluation of some aspects of zinc leaching show that the native bacteria A. ferrooxidans, which is enriched with a 9K Silverman medium under the optimum conditions of pH 2.0, 20 g/L pulp density, and 40 g/L FeSO4, increases the zinc extraction considerably observed by monitoring during15 d, i.e., the zinc concentration has a decrease of about 95% in the iron concentrate.  相似文献   

2.
The effects of sericite particle size, rotation speed, and leaching temperature on sericite dissolution and copper extraction in a chalcopyrite bioleaching system were examined. Finer particles, appropriate temperature and rotation speed for Acidithiobacillus ferrooxidans resulted in a higher Al3+ dissolution concentration. The Al3+ dissolution concentration reached its highest concentration of 38.66 mg/L after 48-d leaching when the sericite particle size, temperature, and rotation speed were -43 μm, 30℃, and 160 r/min, respectively. Meanwhile, the sericite particle size, rotation speed, and temperature can affect copper extraction. The copper extraction rate is higher when the sericite particle size is finer. An appropriately high temperature is favorable for copper leaching. The dissolution of sericite fitted the shrinking core model, 1-(2/3)α-(1-α)2/3=k1t, which indicates that internal diffusion is the decision step controlling the overall reaction rate in the leaching process. Scanning electron microscopy analysis showed small precipitates covered on the surface of sericite after leaching, which increased the diffusion resistance of the leaching solution and dissolved ions.  相似文献   

3.
The comprehensive recovery of small amounts of valuable minerals such as gold and base-metal sulfide minerals from a low-grade refractory ore was investigated. The following treatment strategy was applied to a sample of this ore: gold flotation–gold concentrate leaching–lead and zinc flotation from the gold concentrate leaching residue. Closed-circuit trials of gold flotation yielded a gold concentrate that assayed at 40.23 g·t-1 Au with a recovery of 86.25%. The gold concentrate leaching rate was 98.76%. Two variants of lead-zinc flotation from the residue—preferential flotation of lead and zinc and bulk flotation of lead and zinc—were tested using the middling processing method. Foam from the reflotation was returned to the lead rougher flotation or lead–zinc bulk flotation, whereas middlings from reflotation were discarded. Sulfur concentrate was a byproduct. The combined strategy of flotation, leaching, and flotation is recommended for the treatment of this kind of ore.  相似文献   

4.
碳质金矿石预氧化焙烧堆浸提金的研究   总被引:2,自引:0,他引:2  
介绍了对辽宁丹东某金矿碳质硅化低硫金矿石的焙烧预氧化处理及焙砂直接堆浸的试验研究·分析了不同温度、不同气氛及不同时间条件下的焙砂的氧化状态及影响金浸出率的NaCN的质量分数、喷淋强度、焙砂粒度及喷淋时间等主要因素·实验结果表明,先在450℃,通入少量空气(含氧5%~10%)的条件下,焙烧1h(脱砷),然后,在650℃,通入充足空气的条件下,焙烧2h,矿石中的硫化物和碳物质的氧化率和灰化率分别达98%和97%;当NaCN的质量分数为0 10%~0 15%,喷淋强度为15 0L/(m2·h),焙砂粒度为0~3mm,喷淋时间为8~10天,金的浸出率为84 8%·同时,推荐了焙砂直接堆浸的原则工艺流程...  相似文献   

5.
The iron concentrate from Hercules Mine of Coahuila,Mexico,which mainly contained pyrite and pyrrhotite,was treated by the bioleaching process using native strain Acidithiobacillus ferrooxidans (A.ferrooxidans) to determine the ability of these bacteria on the leaching of zinc.The native bacteria were isolated from the iron concentrate of the mine.The bioleaching experiments were carried out in shake flasks to analyze the effects of pH values,pulp density,and the ferrous sulfate concentration on the bioleaching process.The results obtained by microbial kinetic analyses for the evaluation of some aspects of zinc leaching show that the native bacteria A.ferrooxidans,which is enriched with a 9K Silverman medium under the optimum conditions of pH 2.0,20 g/L pulp density,and 40 g/L FeSO4,increases the zinc extraction considerably observed by monitoring during15 d,i.e.,the zinc concentration has a decrease of about 95% in the iron concentrate.  相似文献   

6.
The magnetic properties of Fe3(1−x)Cr3xC alloys with x=0.05, 0.1, 0.15, and 0.2, which crystallize in the cementite Fe3C-type structure with space group Pnma, were investigated by means of magnetization measurements. These alloys show temperature-induced second-order magnetic phase transitions. The Curie temperature (Tc) of these alloys decreases with increasing x. The isothermal magnetic-entropy changes of these alloys were derived from the magnetic isotherms measured with increasing temperature and increasing field. The maximum values of the magnetic-entropy change are about 0.9 and 3.6 J·kg−1·K−1 at Tc =360 K for x = 0.05 in a magnetic field change from 0 to 1 T and 0 to 5 T, respectively.  相似文献   

7.
Vanadium-bearing titanomagnetite concentrates were desulfurized with Acidithiobacillus ferrooxidans (A. ferrooxidans). The sulfur content of the concentrates was reduced from 0.69wt% to 0.14wt% after bioleaching for 15 d with a 10% pulp density at 30℃. Maintaining a stable pH value during biodesulfurization was critical because of high acid consumption, resulting from a combination of nonoxidative and oxidative dissolution of pyrrhotite in acid solution. It is discovered that the citric acid-disodium hydrogen phosphate buffer of pH 2.0 can control the solution pH value smoothly in the optimal range of 2.0–3.0 for A. ferrooxidans growth. Using the buffer in the volume fraction range of 5.0%–15.0% stimulates A. ferrooxidans growth and improves the biodesulfurization efficiency. Compared with the buffer-free control case, the maximum increase of biodesulfurization rate is 29.7% using a 10.0vol% buffer. Bioleaching provides an alternative process for desulfurization of vanadium-bearing titanomagnetite ores.  相似文献   

8.
Bioleaching was examined for copper extraction from a low grade ore using mesophilic and moderate thermophilic bacteria. Five equal size columns were used for the leaching of the ore. Sulfuric acid solution with a flow rate of 3.12 L·m-2·h-1 and pH 1.5 passed through each column continuously for 90 d. In the first and the second column, bioleaching was performed without agglomeration of the ore and on the agglomerated ore, respectively. 28wt% of the copper was extracted in the first column after 40 d, while this figure was 38wt% in the second column. After 90 d, however, the overall extractions were almost the same for both of them. Bioleaching with mesophilic bacteria was performed in the third column without agglomeration of the ore and in the fourth column on the agglomerated ore. After 40 d, copper extractions in the third and the fourth columns were 62wt% and 70wt%, respectively. Copper extractions were 75wt% for both the columns after 90 d. For the last column, bioleaching was performed with moderate thermophilic bacteria and agglomerated ore. Copper extractions were 80wt% and 85wt% after 40 and 90 d, respectively. It was concluded that crushing and agglomeration of the ore using bacteria could enhance the copper extraction considerably.  相似文献   

9.
Metamaterials such as architected lattice structures have aroused broad interest in being applied as mechanical supports for their lightweight and custom-shaped capabilities.Although various prior efforts have been devoted,a multiscale fabrication of micro-nano lattice structures without penalizing the mechanical properties is still a challenging but highly desirable task.Here we put forward a strategy to produce a mechanically enhanced micro-nano lattice structure by conformally depositing a Co...  相似文献   

10.
The effect of lanthanum ion (La3+) on osteoblast function and cytoskeleton is assessed in vitro. Osteoblasts were isolated from Sprague-Dawley fetal neonatal rats. Cell proliferation and gene expression levels of cbfa-1, alkaline phosphatase (ALP), osteocalcin (OC), bone sialoprotein (BSP) and osteopontin (OPN) were examined by cell counting and RT-PCR. Cytoskeleton F-actin was stained with rhodamine-conjugated phalloidin and was visualized by a confocal microscope. As the results, 10−8-10−4 M La3+-induced osteoblast proliferation on day 2. Data from the RT-PCR assay revealed that 10−6 M La3+ up-regulated the expression levels of ALP, BSP, and cbfa-1 on day 4, while it enhanced the expressions of OC and OPN on day 21. The F-actin cytoskeleton was strengthened and reorganized under the exposure of La3+. In addition, the phosphorylation of focal adhesion kinase (FAK) was significantly promoted in 24 h evaluated by Western blot analysis. These findings indicate that La3+ promotes osteoblast activity through the phosphorylation of FAK and reorganization of the cytoskeleton.  相似文献   

11.
采集广西忻城县红渡镇金银花(Lonicera quaponica)种植示范区人工栽培3年生的金银花样品,测定生物量及各器官的主要元素含量,并估算金银花的经济效益.结果表明,金银花的生物生产力是藤茎(0.79t·hm-2·a-1)>叶子(0.40t·hm-2·a-1)>根(0.33 t·hm-2·a-1)>花(0.30 t·hm-2·a-1);金银花的主要元素(N、P、K)平均含量显示花(5.68 kg·hm-2)>叶子(4.60kg·hm-2)>藤茎(3.06kg·hm-2)>根(2.93 t·hm-2);金银花年均产干花1.78 t·hm-2,年均经济收入每公顷35600元.  相似文献   

12.
LiAlxMn2—xO4 (0≤x≤0.5) was synthesized by high temperature solid-state reaction. The structure and morphology of LiAlxMn2—xO4 were investigated by X-ray diffraction and scanning electron microscopy (SEM). The results indicate that all samples show spinel phase. The polyhedral particles turn to club-shaped, then change to small spherical, and finally become agglomerates with increasing Al content. The supercapacitive performances of LiAlxMn2—xO4 were studied by means of galvanostatic charge-discharge, cyclic voltammetry, and alternating current (AC) impedance in 2 mol·L−1 (NH4)2SO4 aqueous solution. The results show that LiAlxMn2—xO4 represents rectangular shape performance in the potential range of 0-1 V. The capacity and cycle performance can be improved by doping Al. The composition of x=0.1 has the maximum special capacitance of 160 F·g−1, which is 1.37 times that of LiMn2O4 electrode. The capacitance loss of LiAlxMn2—xO4 with x=0.1 is only about 14% after 100 cycles.  相似文献   

13.
A novel hydrothermal process was developed to extract zinc from pure zinc ferrite (ZnFe2O4) nanopowder and zinc-containing electric arc furnace (EAF) dust using hexahydrated ferric chloride (FeCl3·6H2O) as a decomposing agent. The effects of solid FeCl3·6H2O to ZnFe2O4 ratio by mass (RF/Z), hydrothermal reaction temperature, and time on zinc extraction were systematically investigated. In the results, when the hydrothermal reaction is conducted at 150℃ for 2 h with RF/Z of 15:20, the efficiency of zinc extraction from ZnFe2O4 reaches 97.2%, and the concentration of ferric ions (Fe3+) in the leaching solution is nearly zero, indicating a high selectivity for zinc. In addition, the zinc extraction efficiency from the EAF dust reaches 94.5% in the case of the hydrothermal reaction performed at 200℃ for 10 h with the solid FeCl3·6H2O to EAF dust ratio by mass (RF/EAF dust) of 15:10. Zinc and iron separation is achieved by adjusting the pH value of the leaching solution according to the different precipitation pH values of metal hydroxides.  相似文献   

14.
Two different types of chalcopyrite (pyritic chalcopyrite and porphyry chalcopyrite) were bioleached with Acidithiobacillus ferrooxidans ATF6. The bioleaching of the pyritic chalcopyrite and porphyry chalcopyrite is quite different. The copper extraction reaches 46.96% for the pyritic chalcopyrite after 48-d leaching, but it is only 14.50% for the porphyry chalcopyrite. Proper amounts of initial ferrous ions can improve the efficiency of copper extraction for the two different types of chalcopyrite. The optimum dosage of ferrous ions for the pyritic chalcopyrite and porphyry chalcopyrite is different. The adsorption of ATF6 on the pyritic chalcopyrite and porphyry chalcopyrite was also studied in this paper. It is found that ATF6 is selectively adsorbed by the two different types of chalcopyrite; the higher adsorption onto the pyritic chalcopyrite than the porphyry chalcopyrite leads to the higher copper dissolution rate of the pyritic chalcopyrite. In addition, the zeta-potential of chalcopyrite before and after bioleaching further confirms that ATF6 is more easily adsorbed onto the pyritic chalcopyrite.  相似文献   

15.
A new co-precipitation route was proposed to synthesize LiNi0.8Al0.2−xTixO2 (x=0.0-0.20) cathode materials for lithium ion batteries, with Ni(NO3)2, Al(NO3)3, LiOH·H2O, and TiO2 as the starting materials. Ultrasonic vibration was used during preparing the precursors, and the precursors were protected by absolute ethanol before calcination in the air. The influences of doped-Ti content, calcination temperature and time, additional Li content, and ultrasonic vibration on the structure and properties of LiNi0.8Al0.2−xTixO2 were investigated by X-ray diffraction (XRD), scanning electron microscopy (SEM), and charge-discharge tests, respectively. The results show that the optimal molar fraction of Ti, calcination temperature and time, and additional molar fraction of Li for LiNi0.8Al0.2−xTixO2 cathode materials are 0.1, 700°C, 20 h, and 0.05, respectively. Ti doping facilitates the formation of the α-NaFeO2 layered structure, and ultrasonic vibration improves the electrochemical performance of LiNi0.8Al0.2−xTixO2.  相似文献   

16.
The hydrometallurgical strategy of extracting Mn from low-grade Mn ores has attracted attention for the production of electrolytic manganese metal (EMM). In this work, the reductive dissolution of low-grade MnO2 ores using toxic nitrocellulose acidic wastewater (NAW) as a reductant was investigated for the first time. Under the optimized conditions of an MnO2 ore dosage of 100 g·L-1, an ore particle size of -200 mesh, concentrated H2SO4-to-NAW volume ratio of 0.12, reaction temperature of 90℃, stirring speed at 160 r·min-1, and a contact time of 120 min, the reductive leaching efficiency of Mn and the total organic carbon (TOC) removal efficiency of NAW reached 97.4% and 98.5%, respectively. The residual TOC of 31.6 mg·L-1 did not adversely affect the preparation of EMM. The current process offers a feasible route for the concurrent realization of the reductive leaching of Mn and the treatment of toxic wastewater via a simple one-step process.  相似文献   

17.
研究NH3-(NH4)2SO4体系pH、总氨浓度、液固比、温度、矿物粒径、搅拌速度等因素对兰坪低品位氧化锌矿中锌及主要杂质元素浸出行为的影响,并在较低pH和总氨浓度条件下,采用二段逆流浸出工艺对该矿进行处理。实验结果表明:pH、总氨浓度、液固比是影响锌及杂质浸出的主要因素,浸出液中硅、铁、镉、铅等杂质离子的含量都较低。在浸出剂总氨浓度为3 mol/L,pH为9.60,液固比为4,反应时间为4 h的条件下,通过二段逆流浸出工艺处理,锌的浸出率>90%,浸出液pH<9.0,能很好地满足萃取工序的处理要求。  相似文献   

18.
Based on detailed studies, this paper proposesthat in the Tarim Basin, hydrocarbon reservoirs widespreadeither in vertical sequences or in plane and high-porosity andhigh-permeability reservoirs are developed all over the basin.However, obvious difference and heterogeneity exist amongdifferent kinds of reservoirs. The lithologic characteristics,reservoir space types and reservoir properties in variousstrata have been probed. The result indicates that althoughthe Paleozoic carbonates have been deeply buried for a longperiod, high-quality reservoirs with the porosity of up to 5%—8% (12% as the maximum) and the permeability of10×10-3—100×10-3 μm2 (1000×10-3 μm2 as the maximum)can be found in certain areas. These include the area withthe development of reefs and carbonate beaches, the weath-ered-crust buried-hill belts that have undergone thelong-term exposure, weathering and leaching, the area withthe development of dolomitization, and those areas that haveexperienced the resolution of carbonic acid and organic acidgenerated by the maturity of the organic matter. Finally, thegenesis of the high-porosity and high-permeability reservoirsin deep-buried conditions (with the depth more than 3500 m)have been investigated thoroughly.  相似文献   

19.
研究了异丙醇水溶液与(NH4)2SO4的双水相体系下,螯合剂PAN(1-(2-吡啶偶氮)-2-萘酚)与Ni 2+以及吐温80形成的缔合物在两相间的分配行为.结果表明,该缔合物的最大吸收波长为562nm,与PAN和异丙醇水溶液的混合液相比,最大吸收发生了97nm红移.应用该缔合物体系分离测定镍时,其线性范围为0.10~0.60mg/L,线性相关系数为0.999 2,表观摩尔吸光系数为1.7×105 L·mol-1·cm-1.利用该方法萃取测定Ni(Ⅱ)时,干扰离子铅(Ⅱ)、锌(Ⅱ)、铝(Ⅲ)、锰(Ⅱ)、钼(Ⅶ)、Fe(Ⅲ)、铬(Ⅶ)不被萃取,实现Ni(Ⅱ)与上述干扰离子的分离.  相似文献   

20.
三种速生人工林凋落物的持水性能   总被引:1,自引:0,他引:1  
在广西国营高峰林场界牌分场选择立地条件、营林和管理措施、林分长势基本一致的5年生尾巨桉无性系3229(Eucalyptus3229)、厚荚相思(Acaciac rassicarpa)和马占相思(Acacia mangium)速生人工林,采集林下凋落物测定单位面积储量、持水量、持水率和持水速率,研究3种速生树种人工林下凋落物的持水性能。结果表明,厚荚相思凋落物的持水量和持水率最大,分别达18.40×103kg.hm-2和70%,尾巨桉3229的次之,分别为17.34×103kg.hm-2和50%,马占相思的最小,分别是13.49×103kg.hm-2和45%。厚荚相思和尾巨桉无性系3229的持水性能比马占相思的强。  相似文献   