1.
改性纳米碳酸钙补强NR/SBR/BR并用胶的表征   总被引:1,自引:0,他引:1  
通过固相法在硬脂酸改性商品纳米碳酸钙CCR中加入间苯二酚与六亚甲基四胺的络合物RH,制备了改性纳米碳酸钙M-CCR,并分别制备了天然橡胶/丁苯橡胶/顺丁橡胶并用胶与M-CCR和CCR的复合材料.利用橡胶加工分析仪(RPA)和透射电子显微镜(TEM)研究了M-CCR和CCR在并用胶基体中的分散性、界面结合力、加工性能和形态.同时比较了复合材料的力学性能.结果表明,并用胶填充M-CCR的加工性能、补强作用以及填料的分散性和界面结合力均明显优于CCR.  相似文献   

2.
天然橡胶/改性气相法白炭黑纳米复合材料的制备   总被引:2,自引:0,他引:2  
用间苯二酚与六亚甲基四胺络合物(RH)对气相法白炭黑进行表面改性,产物与天然橡胶混合,通过混炼和硫化制备了天然橡彬改性气相法白炭黑(NR/M-silica)纳米复合材料.采用力学性能测试、交联密度测定、透射电镜、差示扫描量热、红外光谱和X射线光电子能谱等手段研究了该纳米复合材料的结构和性能,并探讨了RH改性气相法白炭黑补强天然橡胶的机理.结果表明:M-silica对NR硫化胶的补强效果明显优于未改性的气相法白炭黑,当M-silica用量为4%-10%时,硫化胶的力学性能最佳;M-silica在橡胶基体中分散良好,硫化胶的交联密度和玻璃化温度升高;在改性剂RH作用下,白炭黑中的Si-O键和硅羟基的红外光谱特征吸收峰发生明显的蓝移,且O原子的结合能发生明显的变化,表明白炭黑表面的硅羟基与RH受热后形成的间苯二酚甲醛树脂中的酚羟基之间形成了明显的氢键作用.  相似文献   

3.
混炼插层法制备天然橡胶/蒙脱土纳米复合材料   总被引:8,自引:0,他引:8  
采用有机改性蒙脱土和新型补强性促进剂,通过混炼插层法制备了天然橡胶/蒙脱土纳米复合材料,用X射线衍射和透射电镜表征了纳米复合材料的结构和形态,用表观交联密度测定和红外光谱研究了蒙脱土与橡胶的相互作用,同时用X射线衍射法研究了混炼和硫化过程中天然橡胶分子链对蒙脱土的插层过程.结果表明,蒙脱土在橡胶基体中以纳米级厚度片层分散;补强性促进剂能加强蒙脱土与橡胶间的结合;天然橡胶分子链在混炼过程中便开始对蒙脱土进行插层,并主要在焦烧时间前的硫化诱导期内完成大部分插层过程,硫化开始后蒙脱土的纳米级分散进一步完善,直至硫化完成.添加2%~10%有机蒙脱土的天然橡胶/蒙脱土纳米复合材料的力学性能和动态力学性能优于40%N770炭黑补强的硫化胶.  相似文献   

4.
用间苯二酚与六亚甲基四胺络合物(RH)对气相法白炭黑进行表面改性,通过混炼和硫化制备了天然橡胶/改性气相法白炭黑(NR/M-silica)纳米复合材料,并通过力学性能测试、交联密度测定、透射电镜、差示扫描量热法、红外光谱和X射线光电子能谱等手段研究了纳米复合材料的结构和性能.结果表明:M-silica对NR硫化胶的补强效果显著优于未改性的气相法白炭黑,当M-silica用量为4~10份时,硫化胶的力学性能最佳;M-silica在橡胶基体中分散良好,硫化胶的交联密度和玻璃化温度提高;在改性剂RH作用下,白炭黑的Si-O键和硅羟基的红外光谱特征吸收峰发生明显的蓝移,且O原子的结合能发生明显的变化,表明白炭黑表面的硅羟基与RH受热后形成的间苯二酚甲醛树脂中的酚羟基之间形成了明显的氢键作用.在上述研究的基础上讨论了RH改性气相法白炭黑补强天然橡胶的机理.  相似文献   

5.
研究了过氧化物硫化体系下,甲基丙烯酸镁(MDMA)、炭黑(CB)/MDMA补强天然橡胶的力学性能和交联密度.利用X射线衍射(XRD)证明了:在天然橡胶混炼过程中,氧化镁(MgO)和甲基丙烯酸(MAA)通过中和反应原位生成甲基丙烯酸镁.研究表明:MDMA和CB/MDMA可以有效地补强天然橡胶.交联密度的测定暗示NR/CB/MDMA和NR/MDMA硫化胶的离子键交联密度有着密切的联系,CB和MDMA的并用导致了离子键交联密度的增加,进而对天然橡胶硫化胶产生了协同补强效果.  相似文献   

6.
纳米高岭土和白炭黑硫化橡胶复合材料   总被引:9,自引:0,他引:9  
采用硫化和机械性能测试以及热重分析(TGA)和透射电子显微镜(TEM)等手段,对纳米高岭土(NK)和白炭黑(PS)各自填充的丁苯橡胶(SBR)、天然橡胶(NR)、顺丁橡胶(BR)、三元乙丙橡胶(EPDM)等四种复合材料的硫化性能、力学性能、热稳定性能和微观结构进行了表征和时比.结果表明,纳米高岭土有效改善了橡胶前期硫化的操作安全性,加快了硫化速度,提高了生产效率.其橡胶复合材料具有优异的弹性,拉伸性能与白炭黑橡胶基本接近,撕裂强度和定伸强度比白碳黑稍差.纳米高岭石在橡胶基体中分散性良好,片层厚度小于100 nm,呈定向平行排列.纳米高岭石粒子与橡胶大分子之间良好的界面结合,是促进其热稳定性能提高的主要原因.图5,表3,参11.  相似文献   

7.
研究4种偶联剂KH-560,KH-570,Si-69,C800与白炭黑补强体系在天然橡胶(natural rubber,NR)中的应用,同时探讨偶联剂的种类和用量对NR硫化胶性能的影响.结果表明:随着偶联剂用量的增加,硫化时间缩短,其中偶联剂C800与白炭黑共混提高了NR硫化胶的抗焦烧性能,改善了加工性能;不同的偶联剂对硫化胶的力学性能有不同程度的提高,其中偶联剂KH-560与白炭黑共混增强NR力学性能的效果最好,当KH-560用量为2份时,胶料的力学性能达到最佳效果.  相似文献   

8.
白炭黑(主要成分为纳米SiO2,nano-SiO2)由于易于制取、绿色环保等优点,现被广泛用于橡胶补强中,但是白炭黑因为结构上的特点,导致其在橡胶中的分散性和补强能力比炭黑差。利用硅烷偶联剂改善白炭黑在橡胶中的分散性,并研究改性白炭黑和石墨烯(GE)的协同补强作用对天然橡胶(NR)的影响。使用助分散剂单宁酸(TA)修饰的石墨烯与使用硅烷偶联剂KH570改性的白炭黑通过迈克尔加成反应得到杂化填料(KS-TGE),与天然橡胶充分混合制得KS-TGE/NR复合材料。经过测试,白炭黑经过改性后不仅改善了其在橡胶中的分散性,并且其和石墨烯制得的杂化填料与天然橡胶共混后,天然橡胶的力学性能得到提升。与未改性的nano-SiO2/NR相比,改性后的复合材料拉伸强度最高提升36.3%,断裂伸长率最高提升79.5%,此外KS-TGE/NR仍能保持优异的弹性和动态力学性能。  相似文献   

9.
以镧和维生素C为原料制备了一种新型稀土配合物,将该新型稀土配合物作为一种新型防老剂应用于天然橡胶/炭黑(NR/CB)复合材料中,研究了该稀土配合物对NR/CB混炼胶硫化特性和硫化胶力学性能的影响,通过红外光谱、力学性能保持率及表面形貌变化详细分析了该稀土配合物对NR/CB硫化胶耐老化性能的影响,并与常用橡胶防老剂4010NA、RD和MB进行了比较.结果表明:维生素C-稀土配合物对NR/CB混炼胶具有一定的硫化促进作用,并能提高NR/CB硫化胶的力学性能;维生素C-稀土配合物在NR/CB复合材料中有优良的抗老化作用,其抗热氧老化和抗紫外光老化效果与4010NA、RD相近,优于MB,其抗臭氧老化性能尤为突出,显著优于RD、MB和具有突出抗臭氧性能的4010NA.  相似文献   

10.
研究了稀土异戊橡胶(Nd-IR)和天然橡胶(NR)的共混比对其硫化性能及力学机械性能的影响.研究结果表明:随着Nd-IR用量的增加,Nd-IR/NR共混胶的焦烧时间延长,硫化安全性提高;Nd-IR/NR共混硫化胶的拉伸强度、定伸应力和弹性以及老化后性能率略有下降,硬度(邵尔A)、断裂伸长率和磨耗性能有所提高;电子扫描显微镜(SEM)对共混胶形态分析表明,炭黑在Nd-IR/NR共混橡胶中均匀分散,没有出现团聚和微相分离现象.  相似文献   

11.
纳米微晶纤维素替代炭黑补强天然橡胶   总被引:3,自引:0,他引:3  
采用纳米微晶纤维素(NCC)部分替代炭黑,制备了天然橡胶/纳米微晶纤维素/炭黑复合材料(NR/NCC/CB),研究了NCC对NR/CB复合材料性能的影响.结果表明,NCC提高了CB补强NR的扯断伸长率,并保持在500%以上,永久变形下降至30%以下,且NR/NCC/CB的拉伸强度和撕裂强度基本保持或略优于NR/CB,硬度则基本保持不变;NCC替代炭黑的量为5phr~20phr时,材料仍能保持良好的耐磨耗性能;NCC替代炭黑的量低于15phr时,材料的抗曲挠龟裂性能得到改善;NCC的加入还改善了材料的热空气老化性能,降低了材料的压缩疲劳生热,当NCC取代CB的量为10 phr时,复合材料的生热达到最低值13.0℃.  相似文献   

12.
The N-methyl-D-aspartate subtype of glutamate receptor (NMDAR) serves critical functions in physiological and pathological processes in the central nervous system, including neuronal development, plasticity and neurodegeneration. Conventional heteromeric NMDARs composed of NR1 and NR2A-D subunits require dual agonists, glutamate and glycine, for activation. They are also highly permeable to Ca2+, and exhibit voltage-dependent inhibition by Mg2+. Coexpression of NR3A with NR1 and NR2 subunits modulates NMDAR activity. Here we report the cloning and characterization of the final member of the NMDAR family, NR3B, which shares high sequence homology with NR3A. From in situ and immunocytochemical analyses, NR3B is expressed predominantly in motor neurons, whereas NR3A is more widely distributed. Remarkably, when co-expressed in Xenopus oocytes, NR3A or NR3B co-assembles with NR1 to form excitatory glycine receptors that are unaffected by glutamate or NMDA, and inhibited by D-serine, a co-activator of conventional NMDARs. Moreover, NR1/NR3A or -3B receptors form relatively Ca2+-impermeable cation channels that are resistant to Mg2+, MK-801, memantine and competitive antagonists. In cerebrocortical neurons containing NR3 family members, glycine triggers a burst of firing, and membrane patches manifest glycine-responsive single channels that are suppressible by D-serine. By itself, glycine is normally thought of as an inhibitory neurotransmitter. In contrast, these NR1/NR3A or -3B 'NMDARs' constitute a type of excitatory glycine receptor.  相似文献   

13.
以原代培养的大鼠大脑皮层神经元无镁诱导的反复惊厥样放电为模型,根据对培养6d(天)皮层神经元的不同处理分为3组:正常DMEM培养液组(CONT1)、正常细胞外液组(CONT2)和无镁细胞外液组(MGF)。神经元在上述3种液体中孵育3h,然后恢复正常DMEM培养液继续培养,在培养7、12及17d时应用实时定量PCR测定了发育中大鼠皮层神经元无镁细胞外液处理后NMDA受体亚基NR1、NR2A与NR2B mRNA表达的变化。结果显示: MGF组NR1 mRNA表达在培养7d时明显降低,培养12d时明显升高(p<0.05);NR2A mRNA表达在培养12d时明显降低,培养17d时明显升高(p<0.05);NR2B mRNA表达在培养7d与17d时明显升高(p<0.05)。而培养17d NR1 mRNA表达、7d NR2A mRNA表达及12d的皮层神经元NR2B mRNA表达3组中两两比较无统计学差异(p>0.05)。MGF组NR1/NR2A、NR1/NR2B和NR1/NR2A/NR2B在培养7、12与17d皮层神经元均有明显的变化。可见早期无镁细胞外液处理可以诱导发育中大鼠皮层神经元远期NMDAR亚基mRNA表达的改变。  相似文献   

14.
为了探讨趋化因子MCP-1及其受体CCR2是否参与了SE初期的病理过程,应用SE的匹罗卡品模型,检测SE 30min、SE 1h、SE 2h和SE 1d时,MCP-1及其受体CCR2的mRNA在小鼠海马的表达情况.结果显示,MCP-1及其受体CCR2在小鼠海马组成型表达.与对照组相比,SE 1h时,MCP-1在海马CA1区显著下调(P 0.01);SE 1d时,CCR2在CA3区显著下调(P 0.05).结果说明,MCP-1及其受体CCR2在成年小鼠海马的活动中具有重要的生理功能;MCP-1/CCR2的下调与SE初期病理过程相关,可能由于下调导致了它们的神经保护作用减弱.  相似文献   

15.
用室内模拟培养实验考察纳米TiO2对土壤中硝态氮质量比及硝酸还原酶(nitrate reductase, NR)活性的影响. 结果表明: 纳米TiO2可降低土壤中硝态氮质量比和NR活性, 随着培养时间的增加, 降低程度呈先增加后降低的趋势; 在相同采样时间下, 纳米TiO2在不同土壤中硝态氮质量比和NR活性的降低程度为沙土>黑土>草炭土, 且降低程度随纳米TiO2添加量的增加而增加; 紫花苜蓿使纳米TiO2对土壤中硝态氮质量比和NR活性的降低程度减弱. 因此, 纳米TiO2可降低土壤反硝化作用强度和速率; 紫花苜蓿可降低纳米TiO2的生物毒性.  相似文献   

16.
Salter MG  Fern R 《Nature》2005,438(7071):1167-1171
Injury to oligodendrocyte processes, the structures responsible for myelination, is implicated in many forms of brain disorder. Here we show NMDA (N-methyl-D-aspartate) receptor subunit expression on oligodendrocyte processes, and the presence of NMDA receptor subunit messenger RNA in isolated white matter. NR1, NR2A, NR2B, NR2C, NR2D and NR3A subunits showed clustered expression in cell processes, but NR3B was absent. During modelled ischaemia, NMDA receptor activation resulted in rapid Ca2+-dependent detachment and disintegration of oligodendroglial processes in the white matter of mice expressing green fluorescent protein (GFP) specifically in oligodendrocytes (CNP-GFP mice). This effect occurred at mouse ages corresponding to both the initiation and the conclusion of myelination. NR1 subunits were found mainly in oligodendrocyte processes, whereas AMPA (alpha-amino-3-hydroxy-5-methyl-4-isoxazole propionic acid)/kainate receptor subunits were mainly found in the somata. Consistent with this observation, injury to the somata was prevented by blocking AMPA/kainate receptors, and preventing injury to oligodendroglial processes required the blocking of NMDA receptors. The presence of NMDA receptors in oligodendrocyte processes explains why previous studies that have focused on the somata have not detected a role for NMDA receptors in oligodendrocyte injury. These NMDA receptors bestow a high sensitivity to acute injury and represent an important new target for drug development in a variety of brain disorders.  相似文献   

设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号