45钢盘条冷拔横向裂纹原因分析
引用本文:秦凤婷,宋玉安,晁霞,王红伟.45钢盘条冷拔横向裂纹原因分析[J].济源职业技术学院学报,2012,11(2):34-37,62.
作者姓名:秦凤婷  宋玉安  晁霞  王红伟
作者单位:1. 济源职业技术学院,河南济源,454650
2. 济源钢铁集团,河南济源,454650
摘    要:利用金相显微镜和扫描电镜分析仪对45钢盘条拉拔断裂试样进行了检验与分析,有针对性地寻找出了造成45钢盘条在拉拔过程中出现横向裂纹的主要原因,并提出了合理的工艺改进措施.

关 键 词:45钢  盘条  冷拔  裂纹  原因

Cause for Transverse Cracks by Cold Drawing of 45 Steel Wire Rod
QIN Feng-ting , SONG Yu-an , CHAO Xia , WANG Hong-wei.Cause for Transverse Cracks by Cold Drawing of 45 Steel Wire Rod[J].JOurnal of Jiyuan Vocational and Technical College,2012,11(2):34-37,62.
Authors:QIN Feng-ting  SONG Yu-an  CHAO Xia  WANG Hong-wei
Institution:1(1.JiYuan Vocational and Technical college,Jiyuan 454650,Henan; 2.JiYuan Iron and Steel(Group) CO.LTD.,Jiyuan 454650,Henan)
Abstract:On the base of testing by TEM and SEM of Fracture specimens of 45# steel wire rod,the main causes for transverse cracking of 45# steel wire rode during cold drawing process is found out and corresponding improvement measures are put forward.
Keywords:45# steel  wire rod  cold drawing  cracks  cause