首页 | 本学科首页   官方微博 | 高级检索  
     检索      

临江羚羊铁矿石深度还原试验研究
引用本文:李艳军,韩跃新,朱一民,刘杰.临江羚羊铁矿石深度还原试验研究[J].东北大学学报(自然科学版),2012,33(1):137-140.
作者姓名:李艳军  韩跃新  朱一民  刘杰
作者单位:东北大学资源与土木工程学院,辽宁沈阳,110819
基金项目:国家高技术研究发展计划项目,中国地质调查局科研基金资助项目
摘    要:针对原矿品位为34.79%的吉林临江羚羊铁矿石,进行了深度还原单因素条件试验;考察了还原温度、还原时间、料层厚度等因素对深度还原及磁选分离结果的影响.试验结果表明,还原温度、还原时间对深度还原过程的影响较大.在配煤过剩倍数2.0,还原煤粒度-1.5 mm和矿石粒度-2.0 mm的条件下,适宜的深度还原条件为还原温度1 275℃,还原时间50 min,料层厚度30 mm.在该试验条件下,获得了最终产品含铁质量分数93.05%,回收率85%,金属化率91.29%,达到我国炼钢用直接还原铁H92产品标准要求.

关 键 词:羚羊铁矿石  深度还原  高效分选  铁颗粒  难选铁矿石  

Deep Reduction Tests of Antelope Iron Ore in Linjiang Area
LI Yan-jun,HAN Yue-xin,ZHU Yi-min,LIU Jie.Deep Reduction Tests of Antelope Iron Ore in Linjiang Area[J].Journal of Northeastern University(Natural Science),2012,33(1):137-140.
Authors:LI Yan-jun  HAN Yue-xin  ZHU Yi-min  LIU Jie
Institution:(School of Resources & Civil Engineering,Northeastern University,Shenyang 110819,China.)
Abstract:Deep reduction single factor condition tests on antelope iron ore with the grade of 34.79% from Linjiang area in Jilin Province were conducted,and effect of the factors such as reduction temperature,reduction time and thickness of feed layer on deep reduction and magnetic separation result was investigated.The results indicated that reduction process is considerably influenced by reduction temperature and reduction time.Optimal conditions are as follow: reduction temperature 1 275 ℃,reduction time 50 min,thickness of feed layer 30 mm,excess coal blending multiples 2.0,reduction coal particle size-1.5 mm,and ore particle size size-2.0 mm.Under these conditions,final product with content of Fe 93.05%,recovery 85% and metallization rate 91.29% is obtained,which meets the H92 standard requirement of direct reduction iron product of steelmaking field in China.
Keywords:antelope iron ore  deep reduction  efficient separation  iron particle  refractory iron ores
本文献已被 CNKI 万方数据 等数据库收录!
点击此处可从《东北大学学报(自然科学版)》浏览原始摘要信息
点击此处可从《东北大学学报(自然科学版)》下载免费的PDF全文
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号