Study on high efficient electric discharge milling of silicon carbide ceramic with high resistivity
Authors:RenJie Ji  YongHong Liu  LiLi Yu  XiaoPeng Li  Xin Dong
Institution:(1) College of Electromechanical Engineering, China University of Petroleum, Dongying, 257061, China
Abstract:A new method which employs a group pulse power supply for electric discharge milling of the silicon carbide ceramic with the resistivity of 500 Ω·cm is presented. Due to the good machining stability and high pulse utilization, the material removal rate (MRR) can reach 72.9 mm3/min. The effects of high-frequency pulse duration, high-frequency pulse interval, peak voltage, peak current, polarity, rotate speed and group frequency on the process performance have been investigated. Also the EDMed surface microstructure is examined with a scanning electron microscope (SEM), an X-ray diffraction (XRD), an energy dispersive spectrometer (EDS) and a micro hardness tester. The results show that the conditions of smaller high-frequency pulse duration and pulse interval, higher peak voltage and peak current, and positive tool polarity are suitable for machining the SiC ceramic. The optimal rotate speed is 1090 r/min and the preferable group frequency is 730 Hz. In addition, there is a small quantity of iron on machined surface when machining with steel electrode. The average grain size of the EDMed surface is smaller than that of the unprocessed, and the micro hardness of machined surface is superior to that of the unprocessed. Supported by the National Natural Science Foundation of China (Grant No. 50675225) and Scientific and Technological Project in Shandong Province (Grant No. 2006GG2204001)
Keywords:EDM  silicon carbide ceramic  milling  high resistivity  high efficiency
本文献已被 维普 SpringerLink 等数据库收录!
点击此处可从《中国科学通报(英文版)》浏览原始摘要信息
点击此处可从《中国科学通报(英文版)》下载免费的PDF全文
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号