Leaching of vanadium,sodium, and silicon from molten V-Ti-bearing slag obtained from low-grade vanadium-bearing titanomagnetite |
| |
Authors: | Yuan-yuan Zhu Ling-yun Yi Wei Zhao De-sheng Chen Hong-xin Zhao Tao Qi |
| |
Affiliation: | 1. University of Chinese Academy of Sciences, Beijing 100049, China;2. National Engineering Laboratory for Hydrometal urgical Cleaner Production Technology, Institute of Process Engineering, Chinese Academy of Sciences, Beijing 100190, China |
| |
Abstract: | The water leaching process of vanadium, sodium, and silicon from molten vanadium-titanium-bearing (V-Ti-bearing) slag obtained from low-grade vanadium-bearing titanomagnetite was investigated systematically. The results show that calcium titanate, sodium aluminosilicate, sodium oxide, silicon dioxide and sodium vanadate are the major components of the molten V-Ti-bearing slag. The experimental results indicate that the liquid-solid (L/S) mass ratio significantly affects the leaching process because of the respective solubilities and diffusion rates of the components. A total of 83.8%of vanadium, 72.8%of sodium, and 16.1%of silicon can be leached out via a triple counter-current leaching proc-ess under the optimal conditions of a particle size below 0.074 mm, a temperature of 90°C, a leaching time of 20 min, an L/S mass ratio of 4:1, and a stirring speed of 300 r/min. The kinetics of vanadium leaching is well described by an internal diffusion-controlled model and the apparent activation energy is 11.1 kJ/mol. The leaching mechanism of vanadium was also analyzed. |
| |
Keywords: | titanomagnetite vanadium metallurgy leaching kinetics sodium silicon leaching rate |
本文献已被 万方数据 SpringerLink 等数据库收录! |
| 点击此处可从《矿物冶金与材料学报》浏览原始摘要信息 |
|
点击此处可从《矿物冶金与材料学报》下载免费的PDF全文 |
|