摘    要:将热塑性聚醚酯弹性体(TPEE)和丙烯酸酯橡胶(ACM)共混动态硫化制成一种耐油、耐热的热塑性硫化胶(TPEE/ACM TPVs),并在制备TPEE/ACM TPVs的过程中添加不同量的纳米SiO2,研究了TPEE/ACM共混比和纳米SiO2对TPEE/ACM TPVs动态力学性能、流变性能、力学性能、热稳定性能、耐热老化性能和耐热油性能的影响.研究结果表明:当TPEE/ACM共混比为60/40时,TPVs的综合性能较好;纳米SiO2使TPVs的加工性能变差;TPVs只有一个玻璃化转变温度,纳米SiO2提高了TPVs的玻璃化转变温度;当纳米SiO2添加量为20%(质量分数)时,TPVs的综合力学性能较好;当纳米SiO2添加量为10%或20%时,TPVs的耐热老化性能和耐热油性能较好.

关 键 词:TPEE/ACM热塑性硫化胶  动态硫化  纳米SiO2  流变性能  耐热油性能

Preparation of TPEE/ACM/Nano-SiO2 Composite via Dynamic Vulcanization
Lu Xun , Lin Yan-mei , Wu Shu-qing , Tian Ming.Preparation of TPEE/ACM/Nano-SiO2 Composite via Dynamic Vulcanization[J].Journal of South China University of Technology(Natural Science Edition),2012,40(7):135-141.
Authors:Lu Xun  Lin Yan-mei  Wu Shu-qing  Tian Ming
Institution:Lu Xun Lin Yan-mei Wu Shu-qing Tian Ming(School of Materials Science and Engineering,South China University of Technology,Guangzhou 510640,Guangdong,China)
Abstract:By using thermoplastic polyeher ester elastomer(TPEE) and acrylate rubber(ACM) as the raw materials,thermoplastic vulcanizate composites with oil and thermal resistance,namely TPEE/ACM TPVs,were prepared via a dynamic vulcanization at different nano-SiO2 dosages.Then,the dynamic mechanical property,the rheological behavior,the thermal stability,the heat-aging property and the heat oil resistance of the product were investigated at different TPEE/ACM ratios and nano-SiO2 dosages.The results show that TPEE/ACM TPVs with high performance can be produced when the TPEE/ACM ratio achieves 60/40,that the processability of TPVs becomes poor with the addition of nano-SiO2,that TPVs has only one glass transition temperature that increases after the addition of nano-SiO2,that the TPVs with a nano-SiO2 dosage of 20%(mass fraction) is of high performance,and that better heat-aging property and strong heat oil resistance may obtained when the nano-SiO2 dosage varies from 10% to 20%.
Keywords:TPEE/ACM thermoplastic vulcanizate  dynamic vulcanization  nano-SiO2  rheological behavior  hot oil resistance