Laser ultrasonic visual imaging detection of corrosion damage
Author:
Affiliation:

Fund Project:

  • 摘要
  • |
  • 图/表
  • |
  • 访问统计
  • |
  • 参考文献
  • |
  • 相似文献
  • |
  • 引证文献
  • |
  • 资源附件
  • |
  • 文章评论
    摘要:

    腐蚀损伤广泛存在于国防科技、交通运输等工业领域,严重威胁了结构的安全性和可靠性,因此对腐蚀损伤的安全检测具有重要意义。依据激光超声的基本理论,采用自主设计的全自动激光超声扫描实验系统,通过对铝板中的腐蚀损伤进行激光扫描实验,分析了Lamb波能量、幅值和腐蚀之间的关系,并依据“弹性波能流法”的原理,利用幅值最大值完成了损伤区域的可视化;提出了一种评估铝板腐蚀程度的方法——能量比较法,完成了对不同腐蚀程度的铝板的评估分析。该研究可实现腐蚀缺陷的快速检测与评估,并且检测结果直观可视,展现了巨大的应用前景。

    Abstract:

    Corrosion damage exists extensively in material structures in the industries, such as national defense and transportation, which threatens the safety and reliability of the structure seriously. Therefore, it is of great significance to monitor corrosion damage in materials. In this paper, based on the theory of laser ultrasound, an automatic laser scanner detection system was designed and developed. The laser scanning experiments were carried out on the corrosion damage in the aluminum plate through this system, and the relationship among the Lamb wave energy, amplitude and corrosion was analyzed. The damage area was visualized with the maximum amplitude according to the principle of “elastic wave energy flow method”. Finally, the amplitude integral ratio method was proposed, which can be used to evaluate the degree of corrosion damage. The proposed method can realize the rapid detection and evaluation of corrosion defects with the detection results being visualized, showing a great potential in application.

    参考文献
    相似文献
    引证文献
引用本文

尚晓壮,刘瑶璐,周世杰,宁慧铭,胡宁.腐蚀损伤的激光超声可视化成像检测[J].重庆大学学报,2022,45(12):94-102.

复制
分享
文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:2022-01-22
  • 最后修改日期:
  • 录用日期:
  • 在线发布日期: 2023-01-09
  • 出版日期: